Research Article
Study on Susceptibility and Mechanism of Reheat Cracking in Welded Joint of Type 347 Austenitic Stainless Steel
Figure 13
SEM pictures of fractured SSRT test specimens of welded joints. (a) M-L7 at 750°C, (b) M-L6 at 800°C, (c) M-L4 at 850°C, (d) M-L1 at 900°C.
(a) |
(b) |
(c) |
(d) |