Research Article

The Reinforcement Effect of Nano-Zirconia on the Transverse Strength of Repaired Acrylic Denture Base

Table 2

Mean, standard deviation (SD), and values for different concentrations of glass fiber, zirconia, and nano-zirconia reinforcement.

Mean ± SD Versus HC Versus AP

HC, control83.01 ± 3.03
AP44.85 ± 3.68
2GF56.98 ± 2.580.00010.001
5GF42.75 ± 2.450.00010.175
2ZR50.07 ± 2.970.00010.064
5ZR40.21 ± 3.310.00010.035
2NZR65.43 ± 2.620.0010.0001
5NZR70.77 ± 2.800.0010.0001

Statistical significance of the material with control group only at .
Statistical significance of the material with control as well as AP at .