Research Article

Fracture Resistance of Ceramic Laminate Veneers Bonded to Teeth with Class V Composite Fillings after Cyclic Loading

Table 1

The descriptive data for failure load values of test groups.

Test groupNumberMean (N)Standard deviation (N)Min. (N)Max. (N)95% confidence interval
Lower boundUpper bound

NC11364.28a114.88219.30616.50−296.46432.10
SC11324.57a89.25220.10471.4−271.88377.53
LC10207.26b90.62110.10369.00−151.05263.47

Items in the rows with dissimilar letters are significantly different at 95% level of confidence; avalues are nonsignificantly different at P = 0.81; bvalue is significantly different at P = 0.004.