Reinforcement of PMMA Denture Base Material with a Mixture of ZrO2 Nanoparticles and Glass Fibers

Figure 4

SEM of fracture surfaces of flexural test specimens. (a) Control-0% nano-ZrO2 + 0% GFs; (b) 5% nano-ZrO2 + 0% GFs; (c) 4% nano-ZrO2 + 1% GFs; (d) 3% nano-ZrO2 + 2% GFs.

We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.