Figure 7

SEM of fracture surfaces of impact test specimens. (a) 2.5% nano-ZrO2 + 2.5% GFs; (b) 2% nano-ZrO2 + 3% GFs; (c) 1% nano-ZrO2 + 4% GFs; (d) 0% nano-ZrO2 + 5% GFs.