Compressive strength of samples in Group 1 and 2.
| Group 1 | Group 2 | | Compressive strength (MPa) | | Compressive strength (MPa) |
| Control | 81.92 | Control | 120.16 | Experimental GIC 1 | 81.13 | Experimental GIC 1 | 83.93 | Experimental GIC 2 | 101.85∗ | Experimental GIC 2 | 146.19∗ | Experimental GIC 3 | 63.37 | Experimental GIC 3 | 72.91 | Experimental GIC 4 | 80.46 | Experimental GIC 4 | 117.56 | Experimental GIC 5 | 103.48∗ | Experimental GIC 5 | 157.39∗ | Experimental GIC 6 | 73.76 | Experimental GIC 6 | 93.87∗ |
|
|
∗The symbol indicates that there was significant difference between the experimental GIC and control within the group ( ), n = 6. |