The Corrosion Behaviour of WC-Co-Ru Alloys in Aggressive Chloride Media
Table 6
Raman peak positions (cm−1) found on the surface of WC-Co-Ru/VC alloys after exposure in synthetic mine water solution.
| Sample (wt% Ru) | Raman peaks of samples after exposure to synthetic mine water | Peak 1 | Peak 2 | Peak 3 | Peak 4 | Peak 5 | Peak 6 |
| 0.0 | 1582 | 1232 | — | 598 | 527 | 128 | 0.4 | 1596 | 1337 | — | 581 | 527 | 139 | 1.0 | 1613 | 1374 | 857 | 619 | 520 | 122 | 1.5 | 1586 | 1436 | 867 | 598 | 530 | 152 | 2.0 | 1572 | — | — | 656 | 510 | 186 | 3.0 | 1596 | 1014 | 898 | 625 | 525 | 144 | 0.4VC | 1569 | 1187 | — | 666 | 523 | 190 |
| Average | | | | | | |
|
|