Corrosion rates of unprotected samples after 1 and 2 years.

Sample1-year tests, mm/year2-year tests, mm/year

Corrugated core, face plate0.09 ± 0.010.09 ± 0.01
Corrugated core, inner plate0.13 ± 0.010.09 ± 0.01
Web-core, face plate0.15 ± 0.010.10 ± 0.01
Web-core, inner plate0.13 ± 0.010.10 ± 0.01