Square Wave Voltammetric Determination of Residues of Carbendazim Using a Fullerene/Multiwalled Carbon Nanotubes/Nafion/Coated Glassy Carbon Electrode

Figure 4

Effect of deposition potential on the peak current of 10−6 mol/L MBC, after 10 min preconcentration in 0.01 mol/L acetate buffer (pH 5) and detection in 0.1 mol/L ammoniacal buffer (pH 9). Other experimental conditions as in Figure 2.