Research Article

The Effect of Water on the Tin Electrodeposition from [Bmim]HSO4 Ionic Liquid

Figure 8

XRD patterns of tin deposits obtained from the [Bmim]HSO4/H2O mixture (30% H2O, v/v) solution containing 40 mM SnO at −0.6 V and 353 K for different deposition time: (a) 1 h, (b) 2 h, and (c) 4 h.