ParametersLevel run (N/mm2)

Layer thickness1 (0.075)155.4634.8934.82
254.5734.74
355.0734.82
2  (0.1)458.4635.3435.14
554.5134.73
658.5935.36
3  (0.125)758.6235.3635.34
855.3434.86
961.7335.81

Orientation1  (0°)155.5634.8935.2
458.4635.34
758.6235.36
2  (45°)254.5734.7434.77
554.5134.73
855.3434.86
3  (90°)355.0734.8235.33
658.5935.36
961.7335.81

Hatch spacing1  (0.01)155.5634.8935.04
658.5935.36
855.3434.86
2  (0.015)254.5734.7435.29
458.4635.34
961.7335.81
3  (0.02)355.0734.8234.97
554.5134.73
758.6235.36

We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.