Research Article

Growth of Hierarchically Structured High-Surface Area Alumina on FeCrAl Alloy Wires

Table 1

Weight change for isothermal oxidation at 800°C–1200°C for 16 h.

Weight change (%)

800°C0.03
900°C0.21
1000°C0.53
1200°C0.52