Growth of Hierarchically Structured High-Surface Area Alumina on FeCrAl Alloy Wires

Table 2

EDX data when wire is isothermally oxidised for 16 h at 800°C–1200°C.

AlFeCrOAl/Fe

800°C25.740.114.4180.7
900°C50.69.25.135.15.7
1000°C54.46.93.834.78.1
1200°C55.24.71.838.211.7