Research Article

On the Mechanical Properties of Hybrid Aluminium 7075 Matrix Composite Material Reinforced with SiC and TiC Produced by Powder Metallurgy Method

Figure 3

Sintered samples based on design matrix. (1) 100% of Al, 0% of SiC, and 8% of TiC. (2) 80% of Al, 8% of SiC, and 8% of TiC. (3) 90% of Al, 4% of SiC, and 0% of TiC. (4) 100% of Al, 0% of SiC, and 0% of TiC. (5) 80% of Al, 0% of SiC, and 8% of TiC. (6) 90% of Al, 0% of SiC, and 4% of TiC. (7) 90% of Al, 4% of SiC, and 4% of TiC. (8) 80% of Al, 8% of SiC, and 0% of TiC. (9) 100% of Al, 8% of SiC, and 8% of TiC. (10) 90% of Al, 8% of SiC, and 4% of TiC. (11) 90% of Al, 4% of SiC, and 8% of TiC. (12) 100% Al, 8% of SiC, and 0% of TiC. (13) 80% of Al, 4% of SiC, and 4% of TiC. (14) 100% of Al, 0% of SiC, and 0% of TiC. (15) 100% Al, 4% of SiC, and 4% of TiC.