Microhardness, Structure, and Morphology of Primary Enamel after Phosphoric Acid, Self-Etching Adhesive, and Er:YAG Laser Etching

Table 1

Comparison of Vickers microhardness among groups.

GroupVickers microhardness number ()SDPost hoc test

I198.561.92A
II0.84
III72.341.78C
IV177.766.5A
V59.934.36C

Groups with different letters are significantly different () from each other.