Research Article
Reforming Characteristics under Visible Light Response of Cr- or Ag-Doped Prepared by Sol-Gel and Dip-Coating Process
Table 1
Relationship between each element and different R for Cr-doped TiO2 film.
| R [wt%] | 1 | 10 | 20 | 30 | 40 | 50 | 60 | 70 | 80 | 90 | 100 |
| Element | | | | | | | | | | | | Cr [wt%] | 5.5 | 7.1 | 8.2 | 11.3 | 13.2 | 15.3 | 18.9 | 22.4 | 17.0 | 18.0 | 18.6 | Ti [wt%] | 94.5 | 92.9 | 91.8 | 88.7 | 86.8 | 84.7 | 81.1 | 77.6 | 83.0 | 82.0 | 81.4 |
| Total | 100.0 | 100.0 | 100.0 | 100.0 | 100.0 | 100.0 | 100.0 | 100.0 | 100.0 | 100.0 | 100.0 |
|
|