The specific surface area and porosity of TiO2 by various drying temperature for samples with TiO2 load of 60 g m−2.

Drying temperature °CSpecific surface area m2 g−1Porosity Å

10039.419.4077
15043.358.8541
20049.768.4902
25061.429.1983
30055.358.3969