Research Article

High-Efficiently Photoelectrochemical Hydrogen Production over Zn-Incorporated T i O 2 Nanotubes

Table 1

Surface areas and average pore-diameter for TNT and Zn-TNT calculated by BET method.

BET multipoint surface area [m2gāˆ’1]Total pore volume ( ) [cm3gāˆ’1]Average pore diameter [nm]

TNT104.210.23258.9262
0.001 mol% Zn-TNT118.210.460515.583
0.01 mol% Zn-TNT135.710.42812.615
0.1 mol% Zn-TNT153.010.2937.66