Research Article
Tailoring the Composition and Properties of Sprayed CuSbS2 Thin Films by Using Polymeric Additives
Table 2
Crystallite size and phase composition for samples A–H.
| Sample | Phase composition (%) | Crystallite size (Å) | | Cu3SbS4 | CuSbS2 | Cu3SbS3 | Cu3SbS4 | CuSbS2 | Cu3SbS3 |
| A | 34.2 | 65.8 | — | 236.1 | 143.1 | — | B | 78 | 22 | — | 236.1 | 161.5 | — | C | 30 | 70 | — | 181.9 | 180.1 | — | D | 27 | 73 | — | 146.3 | 164.7 | — | E | 34 | 66 | — | 217.3 | 216.2 | — | F | 67 | 28 | 5 | 196.3 | 171.5 | 352 | G | 82 | 11 | 7 | 172.4 | 173.8 | 577.7 | H | 82 | 11 | 7 | 159.4 | 160.7 | 268.8 |
|
|