Research Article

Optical and Morphological Studies of Thermally Evaporated PTCDI-C8 Thin Films for Organic Solar Cell Applications

Figure 4

X-ray reflectivity curves for (a) different thicknesses of PTCDI-C8 films as well as the measured and simulated reflectivity data for (b) Kiessig fringes and (c) Laue oscillations for PTCDI-C8 film with 27 nm thickness.
205105.fig.004a
(a)
205105.fig.004b
(b)
205105.fig.004c
(c)