Surface roughness of CP-Ti and Ti-153 sheet specimens before hydrogenation.

CP-TiTi-153
(nm) (nm) (nm) (nm)

134.7 ± 3.5166.3 ± 3.8162.6 ± 10.6171.1 ± 15.0

: The arithmetic mean of the departure of the profile from the mean line.
: The root-mean-square parameter corresponding to .