Research Article
Oxidation of 4-Chlorophenol by Mesoporous Titania: Effect of Surface Morphological Characteristics
Table 2
Specific surface area, average pore size, and average crystallite size of mesoporous titania samples with different drying rate in rotary evaporator.
| Drying rate | Calcination (°C) | Sample ID | Specific surface area (m2/g) | Average pore size (nm) | Average crystallite size (nm) |
| Fast | 350 | FR3 | 150 | 3.8 | 8 | 400 | FR4 | 103 | 4.3 | 10 |
| Medium | 350 | MR3 (RB3) | 145 | 4.3 | 8 | 400 | MR4 (RB4) | 108 | 4.9 | 10 |
| Slow | 350 | SR3 | 147 | 4.9 | 8 | 400 | SR4 | 108 | 5.6 | 10 |
|
|