Research Article
Study on Mitigation Method of Solder Corrosion for Crystalline Silicon Photovoltaic Modules
Figure 9
EL images of PV modules: the sample without Al after (a) 0 h, (b) 1000 h, (c) 2000 h, and (d) 2500 h of DH exposure and the sample with Al after (e) 0 h, (f) 1000 h, (g) 2000 h, and (h) 2500 h of DH exposure.
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |
(g) |
(h) |