Research Article

The Structure and Stability of Molybdenum Ditelluride Thin Films

Figure 6

XRD patterns of Mo-Te thin films with thickness of 450 nm annealed at 470°C for different times in N2 ambient.
956083.fig.006a
(a)
956083.fig.006b
(b)
956083.fig.006c
(c)