Selective Removal of Perfluorooctanoic Acid Using Molecularly Imprinted Polymer-Modified TiO2 Nanotube Arrays

Figure 7

(a) PFOA degradation and defluorination towards UV photolysis, TiO2 NTs, NIP-TiO2 NTs, and MIP-TiO2 NTs under 8 h irradiation; (b) release of fluoride ion responded to the change of PFOA concentration in the presence of MIP-TiO2 NTs; (c) trends of total organic carbon responded to the change of PFOA concentration in the presence of MIP-TiO2 NTs. Initial concentrations of PFOA and TOC were 72.5 μmol/L (30 mg/L).
(a)
(b)
(c)