Research Article
Investigation on Potential-Induced Degradation in a 50 MWp Crystalline Silicon Photovoltaic Power Plant
Figure 3
The measured potential difference of 18 modules from the same module string between the ground and the pole of module under an open circuit.
(a) Soon after grid-connection |
(b) After one year of operation |