In Situ Low-Temperature Chemical Bath Deposition of CdS Thin Films without Thickness Limitation: Structural and Optical Properties

Table 3

Thickness and average transmission values of the as-deposited (sample A) and annealed CdS thin films (samples B, C, D, and E).

SampleThickness (nm) (%) (visible region)

A254 ± 482
B251 ± 481
C253 ± 480
D259 ± 479
E219 ± 470