The average values of lifetime, resistivity, and B, O, C, Fe, Cu, and Ni concentrations of five groups of Si wafers.

GroupLifetime (μs)Resistivity (Ω∙cm)B (atoms/cm3)O (atoms/cm3)C (atoms/cm3)Fe (atoms/cm3)Cu (atoms/cm3)Ni (atoms/cm3)

127.601.79
224.191.78
324.171.49
422.951.29
521.571.16