Properties of Natural Rubber-Based Composites Containing Fullerene

Figure 3

TEM micrograph of composites containing 1.5 phr of fullerene (a) and a selected area electron diffraction (SAED) micrograph (b).
967276.fig.003a
(a)
967276.fig.003b
(b)