Effects of polymer yield, reaction time, and product intrinsic viscosity on [M]/[HEMA].

Sample numberTime, h[M]/[HEMA], mol/molYield, %[η], dL/g   (GPC) *

225Control870.5826.71.43
23520850.2116.41.56
24540880.3222.01.63

Reaction conditions: T = 55°C, [M]/[E]—30 wt./wt., [M]—25 wt.%.
The ratio is given for macromolecular peak only, while for the whole sample, the PDI is much higher.