Research Article

Rapid Synthesis of Superabsorbent Smart-Swelling Bacterial Cellulose/Acrylamide-Based Hydrogels for Drug Delivery

Table 2

Mechanical properties of hydrogels ( ).

FormulationCompressive stress
(MPa)
(mean ± SD)
Compressive strain
(mm/mm)
(mean ± SD)
Compressive modulus
(MPa)
(mean ± SD)

PAMa0.434 ± 0.0381.685 ± 0.0831.592 ± 0.069
DHa0.265 ± 0.0251.961 ± 0.0121.449 ± 0.079
0.410 ± 0.0531.359 ± 0.0741.172 ± 0.056
PAMb0.562 ± 0.0671.608 ± 0.0871.237 ± 0.082
DHb0.407 ± 0.0311.464 ± 0.0130.722 ± 0.026
0.304 ± 0.0291.636 ± 0.0930.229 ± 0.014

Compression test of hydrogel with 500% swelling ratio.
bCompression test of hydrogel with equilibrium swelling ratio.