Composition of six polymer-sand composite samples with different weight % of the polymer.
| Sample number | 1 | 2 |
3 | 4 | 5 | 6 |
| Solid PAM g | 0.33 | 0.66 | 0.99 | 1.33 | 1.66 | 1.99 |
| Mix of PAM solution with 300 g of sand | 13 mL | 26 mL | 39 mL | 52 mL | 65 mL | 78 mL |
| Constant H2O % | 2.5 | 2.5 | 2.5 | 2.5 | 2.5 | 2.5 |
| Weight % of PAM in 300 g of sand | 0.11 | 0.22 | 0.33 | 0.44 | 0.55 | 0.66 |
|
|