Research Article

Keggin-Type Heteropolyacid for Ring-Opening Polymerization of Cyclohexene Oxide: Molecular Weight Control

Figure 2

IR spectrum of poly(CHO). Polymerization catalyzed by 0.2 g of H3PW12O40 at 40°C during 3 hours in CH2Cl2.