Effect of Die Head Temperature at Compounding Stage on the Degradation of Linear Low Density Polyethylene/Plastic Film Waste Blends after Accelerated Weathering

Table 4

Colour parameters and total change in colour () for studied formulations at different accelerated weathering exposure (hours) processed at a DHT = 195°C.

Materials (wt.%/wt.%)Exposure duration (hours)

V (100 LLDPE/0 waste)4825.8
7227.0
12028.8
16826.8
21626.2
26429.5
36030.3

B1 (90 LLDPE/10 waste)4828.7
7230.0
12028.2
16826.0
21630.0
26421.9
36029.8

B2 (75 LLDPE/25 waste)4826.0
7224.5
12025.3
16827.0
21626.6
26429.3
36028.6

B3 (50 LLDPE/50 waste)4823.5
7225.1
12025.9
16825.5
21625.0
26428.7

B4 (25 LLDPE/75 waste)4822.3
7221.6
12021.2
16823.6
21622.30
26421.8

B5 (10 LLDPE/90 waste)4818.74
7219.26
12028.22
16826.0
21629.97
26421.94