Research Article
Laser-Based Joining of Thermoplastics to Metals: Influence of Varied Ambient Conditions on Joint Performance and Microstructure
Figure 3
(a) Overlap width is equivalent to weld width (characteristic example for joining speed 4 mm·s−1). (b) Temperature-time profiles from 2 mm·s−1 up to 7 mm·s−1.
(a) |