Microstructure and Mechanical Properties of the Butt Joint in High Density Polyethylene Pipe
Figure 3
SEM images of the tensile fracture surface of W-PE10 (a, b) near to crack initiation point and W-PE10 after etching with potassium permanganate based etchant (c, d). Scale bar is 500 μm (a, c) and 100 μm (b, d).