Research Article
Influence of Fiber Content on Mechanical and Morphological Properties of Woven Kenaf Reinforced PVB Film Produced Using a Hot Press Technique
Table 1
Properties of woven kenaf [
18].
| Characterization | Woven kenaf |
| Thickness, (mm) | 2 ± 0.2 | Weight (g/m2) | 890 | Density (g/cm3) | 1.2 | Warp density (warp/inch) | 12 | Weft density (weft/inch) | 12 | Wavelength, (mm) | 4.2 | Interyarn fabric porosity () | 0.274 | Moisture content (%) | 8.353 | Water uptake (%) | 148.86 | Average breaking strength (MPa) | 100.64 | Average maximum strain (%) | 17.3 |
|
|