International Journal of Polymer Science / 2017 / Article / Fig 8

Research Article

Discoloration Effects of High-Dose γ-Irradiation and Long-Term Thermal Aging of (U)HMW-PE

Figure 8

A block (200 mm × 80 mm × 40 mm) of HMW-PE with black spots that appeared after 31 days of pure thermal aging at 125°C.

We are committed to sharing findings related to COVID-19 as quickly and safely as possible. Any author submitting a COVID-19 paper should notify us at help@hindawi.com to ensure their research is fast-tracked and made available on a preprint server as soon as possible. We will be providing unlimited waivers of publication charges for accepted articles related to COVID-19. Sign up here as a reviewer to help fast-track new submissions.