Preparation of High Modulus Poly(Ethylene Terephthalate): Influence of Molecular Weight, Extrusion, and Drawing Parameters

Table 4

Crystallinity of as-spun PET bristles extruded at 20 rpm and different take-up speeds.

Crystallinity
@Take-up speed
10 m·min−120 m·min−1

() @ Recrystallization peak24.9%25.6%
() @ Melt peak29.4%28.6%
()−()4.5%3.0%