Research Article

Prestress Loss of CFL in a Prestressing Process for Strengthening RC Beams

Table 2

Prestress loss by predictions and measurements during tension.

SpecimensPrestress levels/%/mmPredicted prestress loss/MPaMeasured prestress loss/MPaRelative errors/%

PB-880.434.2833.171.033
PB-15150.651.4350.161.025
PB-22220.869.5768.661.013

Note. PB-8 are prestressed-CFL-strengthened RC beams with 8% prestress level.