Fracture deformation with thickness of hybrid panels after MgSO4 solution immersions.
(a) 9.2 mm (plain) |
(b) 12.2 mm (plain) |
(c) 15.2 mm (plain) |
(d) 9.2 mm (sand blast) |
(e) 12.2 mm (sand blast) |
(f) 15.2 mm (sand blast) |