Research Article
Recycled Polypropylene Improved with Thermoplastic Elastomers
Table 7
Tensile properties for RPP/elastomer compounds and RPP.
| Code compound | Tensile strength at break [MPa] | Elongation at break [%] |
| RPP | 2.06 ± 0.20 | 2.83 ± 0.11 | RPP/SEBS | 7.33 ± 0.70 | 12.89 ± 4.20 | RPP/SIS30 | 11.70 ± 0.77 | 10.96 ± 2.25 | RPP/SIS20 | 8.90 ± 2.20 | 11.03 ± 4.08 |
|
|