Research Article

Rheological Properties in Aqueous Solution for Hydrophobically Modified Polyacrylamides Prepared in Inverse Emulsion Polymerization

Table 1

Viscometric molecular weight for the different polymers synthetized.

MethodSolutionEmulsionEmulsion

Monomer concentration wt%31.504

PolymerMolecular weight (g/mol)
ViscometricViscometricSECViscometric

PAM55933216520 = 137,500
= 506490
466029
PAM-co-DAM80879239777492249
PAM-co-DMA514452
PAM-co-HDAM350763

Monomer concentration is related to total weight of reaction mixture.