Research Article

(Bio)degradable Ionomeric Polyurethanes Based on Xanthan: Synthesis, Properties, and Structure

Table 4

Results of of IPU/Xa incubation in the soil.

Characteristic
(4 months)
Xa content, %
05,010,030,0

Weight loss, %1,310,21338
Changing of physic-mechanical indices after the test (σ/ε), %2,8/1,450,1/18,0

of the film.