Properties of buccal films (mean ± SD, ): percentage of swelling (%), drug content (%), thickness (mm), force (N), puncture strength (N/mm2), elongation break (%), and mucoadhesive strength (N/cm2).

FilmSwellingDrug contentThicknessForcePuncture strengthElongation to breakMucoadhesive strength
%Q%mmNN/mm2%N/cm2

F1320.53 ± 1.08109.60 ± 1.800.119 ± 0.01612.58 ± 0.110.69 ± 0.00625.53 ± 5.533.49 ± 0.05
F2298.93 ± 0.53103.60 ± 4.190.148 ± 0.01510.66 ± 3.240.59 ± 0.17935.98 ± 2.423.68 ± 0.03
F3442.11 ± 2.73110.90 ± 0.130.166 ± 0.01226.35 ± 9.381.45 ± 0.51842.15 ± 2.055.30 ± 0.07
F4438.99 ± 1.74109.30 ± 0.220.242 ± 0.01821.07 ± 1.991.16 ± 0.11049.68 ± 9.115.50 ± 0.06
F5482.99 ± 9.0497.37 ± 1.850.205 ± 0.02931.79 ± 2.951.75 ± 0.16239.59 ± 5.015.47 ± 0.11
F6480.12 ± 7.37103.37 ± 1.250.225 ± 0.02521.17 ± 3.301.39 ± 0.18240.93 ± 2.065.74 ± 0.06
F7540.99 ± 3.35102.01 ± 0.550.233 ± 0.02748.57 ± 12.792.68 ± 0.70731.78 ± 10.147.31 ± 0.07
F8572.70 ± 2.16103.94 ± 1.900.222 ± 0.02148.07 ± 13.132.66 ± 0.72544.00 ± 13.157.57 ± 0.07