Swelling properties and crosslinking densities of the various compounds.
| Samples/parameters | Qr | (cal/cc)1/2 | | (mol/cm3) |
| TP1 | 1.736 | 8.173 | 0.363 | 0.00412 | TP2 | 1.059 | 8.173 | 0.363 | 0.02997 | TP3 | 1.590 | 8.173 | 0.363 | 0.00378 | TP4 | 2.290 | 8.070 | 0.370 | 0.00116 | TP5 | 1.418 | 8.210 | 0.361 | 0.00588 | TP6 | 1.569 | 8.210 | 0.361 | 0.00399 | TP7 | 1.609 | 8.240 | 0.359 | 0.00366 | TP8 | 1.792 | 8.240 | 0.359 | 0.00253 |
|
|