Research Article

Phosphorus Flame Retardants for Polymeric Materials from Gallic Acid and Other Naturally Occurring Multihydroxybenzoic Acids

Table 1

Thermal decomposition of phosphorous esters of gallic acid anilide.

CompoundTemperature of decomposition onset (°C)aTemperature of maximum decomposition rate (°C)Decomposition residue (%)b
NitrogenAirNitrogenAirNitrogenAir

GA-DEP2391752532053713
GA-DOPO316313373366187

aExtrapolated onset temperature from the derivative plot of mass loss versus temperature. bPercentage of the initial sample mass.