Research Article

Fatigue Fracture Properties and Morphology of Polyoxymethylene (POM) Plates Produced under Moderate Processing Conditions

Table 2

Processing parameters used for compression molding (plate dimension: 150 × 150 × 4 mm).

HeatingCompressionCooling

Delrin
Pressure (bar)1100100
Temperature (°C)21021030
Time span (min)161518
Tenac
Pressure (bar)1100100
Temperature (°C)21021030
Time span (min)181518