Research Article

High-Efficiency DNA Extraction Using Poly(4,4-Cyclohexylidene Bisphenol Oxalate)-Modified Microcrystalline Cellulose-Magnetite Composite

Table 2

The values of surface area and pore volume for poly(4,4-cyclohexylidene bisphenol oxalate).

Relative pressure (P/P0)Surface areaBET surface areaSingle-point adsorption total pore volume of pores less than 842.856 Å radiusSingle-point desorption total pore volume of pores less than 928.410 Å radiusPore size (adsorption and desorption average pore diameter) by (4 V/A by BET)

0.2711.4475 m2/g2.6549 m2/g
0.9880.181943 cm3/g
0.9890.198761 cm3/g2,741.2863 Å and 2,994.6726 Å