Research Article
Influence of Four Ageing Methods on the Mechanical Properties of Bamboo Scrimber
Table 5
The decrease of bamboo scrimber mechanical properties after the four accelerated ageing testing treatment methods.
| Degradation of mechanical properties | I (%) | II (%) | III (%) | IV (%) |
| Nail-holding power | | | | | Plane | 41.8 | 4.1 | 10.5 | 9.9 | Side | 39.3 | 8.4 | 17.3 | 13.0 | End face | 65.7 | 5.0 | 48.8 | 27.9 | MOR | 24.2 | 15.0 | 17.5 | 27.2 | MOE | 8.4 | 2.6 | 6.9 | 12.8 | Horizontal shear strength | 16.7 | 3.1 | 11.1 | 11.1 |
|
|